Copper & Copper-Alloys Bare Welding Rods for TIG/MIG welding.

CLASSIFICATION :AWS/SFA A5.7 ERCuSn-C(UNS number C52100)
DESCRIPTION & APPLICATION :

ERCuSn-C filler metal contains about 8% tin and up to 0.35% phosphorus. The higher tin increases strength and wear resistance and increases the solidification temperature range during deposition of the weld metal.When gas tungsten arc welding with ERCuSn-C filler metals, preheating is desirable. Welding is done in the flat position only.

SHIELDING GAS : GMAW: 100% Ar or 75/25 Ar/He; GTAW: 100 % Ar/He
CHEMICAL COMPOSITION %
Cu Zn Sn Fe P Al Pb
Remainder 0.2 7.0-9.0 0.1 0.10-0.35 0.01 0.02
Single value maximum
TYPICAL HARDNESS AND TENSILE STRENGTH :
~Tensile Strength (N/mm2) HBW
380 Min. 85 – 100
DIEMENSION, TYPICAL CURRENT CONDITION & PACKING DATA (RAAJMIG BRONZE -C)
Size(mm) Size(inch) Spool packing 12.5 kg. Spool packing 15 kg Drum packing 100/200kg
1.20 0.047 right right right
1.60 0.0625 right right right
DIEMENSION, TYPICAL CURRENT CONDITION & PACKING DATA(RAAJTIG BRONZE -C)
Size (mm) Size (inch) Length (mm) Length (inch) ~Ampere (DCEN) Tube packing 5 kg Box packing 20 kg
1.6 1/16” 1000 36” 70-120 right right
2 5/64” 1000 36” 100-130 right right
2.40 / 2.50 3/32” 1000 36” 160-220 right right
3.2 1/8” 1000 36” 170-230 right right
4 5/32” 1000 36” 220-300 right right
Customized packing on request.