High Resistance to Abrasion Moderate impact at elevated temperature
Basis OF Alloys : C, Cr, Mn, Ni
Basis OF Alloys : C, Cr, Mn, Ni
CHARACTERISTICS :
Basic coated, Hard facing electrode for achieving high deposition efficiency 170% approx. High resistant to abrasion due to high content of chromium and carbon .machining by grinding. Resistant to heavy mineral abrasion and moderate.
APPLICATION :
- Blast furnace bells & Hooper’s
- Refectory press screws.
- Conveyor screws, cement press crews.
- Dredger bucket screws, bucket teeth & lips.
- Tube mill and Rolling mill guides, pug mill knife.
RE-DRY CONDITION :
Re-Dry the electrode at 250°C-300°C for 1 hour
ALL WELD CHEMICAL COMPOSITION %
C | Mn | Si | Cr | Ni |
5.0 max | 1.00 max. | 2.00 max | 24-28 | 3.50-4.50 |
WELD METAL HARDNESS :
As welded Hardness |
56-62 HRC |
DIMENSION, CURRENT CONDITION & PACKING DATA
Size(mm)(Dia) | Size(inch)(Dia) | Current Condition (DC+/ AC) Amps | weight of packet (Kgs) | Weight of Case |
3.15/ 3.20 X 350 | 1/ 8” X 14” | 100-130 | 5 | 20 |
4.00 X 350 | 5/ 32” X 14” | 150-180 | 5 | 20 |
5.00 X 350 | 3/ 16” X 14” | 210-260 | 5 | 20 |